Polypropylene biaxial geogrid
Classification :
PP Biaxial Geogrid
PRODUCT DETAILS
Keywords:
Polypropylene biaxial geogrid
Description of Polypropylene biaxial geogrid
Polypropylene biaxial geogrid is made in Polypropylene (PP) with their square apertures, high tensile strength and optimised geometry of nodes and ribs make them equal to any other similar material.
PP Plastic Biaxial Geogrids lies mainly in confining soil and increasing its shearing resistance by a process of interlocking between the square ribs and the soil. The load dispersal effect from the interlocking mechanism is highly effective and can reduce sub-base thickness and construction cost.
PP Plastic Biaxial Geogrids can be used with any kind of mechanical fill material. Two aperture size ranges are available for optimum matching with project fill.
Specification of Polypropylene biaxial geogrid:
|
Specification |
Test Method |
|
BX1515 |
BX2020 |
BX2525 |
BX3030 |
BX4040 |
BX1100 |
BX1200 |
BX3030L |
||||||||
|
Index |
|
Unit |
MD |
XMD |
MD |
XMD |
MD |
XMD |
MD |
XMD |
MD |
XMD |
MD |
XMD |
MD |
XMD |
MD |
XMD |
|
Ultimate Tensile strenth |
D6637 |
KN/m |
15 |
15 |
20 |
20 |
25 |
25 |
30 |
30 |
40 |
40 |
12.4 |
19.0 |
19.2 |
28.8 |
30 |
30 |
|
Aperture Size |
|
mm |
39 36 33 31 |
39 36 33 31 |
39 36 33 31 |
39 36 33 31 |
39 36 33 31 |
39 36 33 31 |
39 36 33 31 |
39 36 33 31 |
39 36 33 31 |
39 36 33 31 |
25 |
33 |
25 |
33 |
65 |
65 |
|
Minimum Rib Thickness |
|
mm |
1.0 |
0.8 |
1.5 |
1.1 |
1.8 |
1.4 |
2.2 |
1.7 |
2.5 |
2.0 |
1.0 |
0.8 |
1.4 |
1.27 |
1.7 |
1.5 |
|
Tensile Strength @2% Strain |
D6637 |
KN/m |
6 |
6 |
7 |
7 |
9 |
9 |
11 |
11 |
15 |
15 |
4.1 |
6.6 |
6 |
9 |
11 |
11 |
|
Tensile Strength @5% Strain |
D6637 |
KN/m |
11 |
11 |
13 |
13 |
17 |
17 |
21 |
21 |
27 |
27 |
8.5 |
13.4 |
11.8 |
19.6 |
21 |
21 |
|
Junction Efficiency |
|
% |
95 |
95 |
95 |
95 |
95 |
95 |
95 |
95 |
||||||||
|
Flexural Stiffness |
D7748 |
mg-cm |
690,000 |
780,000 |
860,000 |
960,000 |
1,000,000 |
250,000 |
750,000 |
960,000 |
||||||||
|
Aperture Stability |
|
m-N/deg |
0.30 |
0.50 |
0.62 |
0.75 |
0.85 |
0.32 |
0.65 |
0.75 |
||||||||
|
Resistance to Installation Damage |
|
%SC/%SW/%GP |
95/93/90 |
95/93/90 |
95/93/90 |
95/93/90 |
95/93/90 |
95/93/90 |
95/93/90 |
95/93/90 |
||||||||
|
Resistance to Long Term Degradation |
|
% |
100 |
100 |
100 |
100 |
100 |
100 |
100 |
100 |
||||||||
|
Resistance to UV Degradation |
D4355 |
% |
100 |
100 |
100 |
100 |
100 |
100 |
100 |
100 |
||||||||
|
Minimum Cabon Black |
|
% |
2 |
2 |
2 |
2 |
2 |
2 |
2 |
2 |
||||||||
|
Unit Weight |
|
g/m2 |
175-210 |
220-250 |
260-300 |
300-340 |
450-500 |
180-210 |
280-310 |
320-360 |
||||||||
|
Rolls Dimensions (Length, Width) |
|
m |
100*3.95 100*5 100*5.95 |
50*3.95 50*5 50*5.95 |
50*3.95 50*5 50*5.95 |
50*3.95 50*5 50*5.95 |
50*3.95 |
75*3.95 75*5 75*5.95 |
50*3.95 50*5 50*5.95 |
50*3.95 50*5 50*5.95 |
||||||||
Application:

Shipping packaging:
PP Plastic Biaxial Geogrid
Packing Details : White or Yellow tape. We provide OEM mark.

CUSTOMER VISIT
FAQ
Q
Q: What happens if the product is damaged during transportation?
A
Q
Q: What trade terms and payment methods do you accept?
A
Q
Q: Can you provide samples?
A
Q
Q: What are the production cycle and delivery time?
A
Q
Q: How should the product be packaged? Is it suitable for sea freight?
A
Q
Q: What is the minimum order quantity (MOQ)?
A
Packaging and shipping